| dc.contributor.author | Mutsata, K. | ru |
| dc.contributor.author | Govha, J. | ru |
| dc.contributor.author | Musiiwa, P. B. | ru |
| dc.contributor.author | Moyo, L. | ru |
| dc.coverage.spatial | Минск | ru |
| dc.date.accessioned | 2026-01-14T07:23:13Z | |
| dc.date.available | 2026-01-14T07:23:13Z | |
| dc.date.issued | 2025 | |
| dc.identifier.citation | Sustainable recovery of high-purity amorphous silica from local sand deposits in Zimbabwe using citric acid leaching pre-treatment = / K. Mutsata, J. Govha, P. B. Musiiwa, L. Moyo// Приборостроение-2025 : материалы 18-й Международной научно-технической конференции, 13–15 ноября 2025 года Минск, Республика Беларусь / редкол.: А. И. Свистун (пред.), О. К. Гусев, Р. И. Воробей [и др.]. – Минск : БНТУ, 2025. – С. 412-414. | ru |
| dc.identifier.uri | https://rep.bntu.by/handle/data/162695 | |
| dc.description.abstract | This study presents an alternate process for utilization of Zimbabwean silica sand to produce high-purity amorphous silica. The objective was to develop an optimum multi-stage purification that is environmentally friendly. The methodology starts with pre-treatment step with hydrochloric acid, followed by citric acid chelation stage to remove metallic oxide impurities. The pre-treated silica sand was then converted into sodium silicate intermediate through digestion with sodium hydroxide, from which high-purity silicic acid was precipitated using sulfuric acid. Studies on the chelation stage identified the optimal conditions for maximum impurity removal as a citric acid concentration of 4 M , a leaching duration of 4 hours, and a solid-to-liquid ratio of 1:4, all conducted at a temperature of 90 °C . Under these conditions, 70.3 g of high-purity amorphous silica was obtained from 100 g of silica sand. The results demonstrate that this approach, using organic acid leaching with a chemical conversion and precipitation route, represents a viable and effective pathway for upgrading lower-grade silica resources into a high-value precursor material suitable for semiconductor applications. | ru |
| dc.language.iso | en | ru |
| dc.publisher | БНТУ | ru |
| dc.title | Sustainable recovery of high-purity amorphous silica from local sand deposits in Zimbabwe using citric acid leaching pre-treatment | ru |
| dc.type | Working Paper | ru |